Petersliner 1
|
Papierparameter
|
 |
Toleranz
|
|
Basis weight
DIN EN ISO 536
|
g/qm
|
125
|
130
|
140
|
150
|
160
|
170
|
180
|
190
|
± 3%
|
|
Bursting resistance (Mullen tester)
|
|
370
|
390
|
420
|
450
|
480
|
510
|
540
|
570
|
- 10%
|
|
Burst factor ISO 2759
|
|
|
 |
|
Short Span Compression Test (SCT) CD
DIN 54 518
|
|
2,10
|
2,20
|
2,40
|
2,55
|
2,70
|
2,85
|
3,05
|
3,20
|
- 0,20
|
Download of the Technical Data in PDF format.
Petersliner 2
|
Papierparameter
|
 |
Toleranz
|
|
Basis weight
DIN EN ISO 536
|
g/qm
|
125
|
130
|
140
|
150
|
160
|
170
|
180
|
190
|
200
|
210
|
220
|
± 3%
|
|
Bursting resistance (Mullen tester)
|
|
320
|
340
|
360
|
390
|
410
|
440
|
470
|
490
|
520
|
540
|
570
|
- 10%
|
|
Burst factor ISO 2759
|
|
|
 |
|
Short Span Compression
Test (SCT) CD
DIN 54 518
|
|
2,05
|
2,15
|
2,30
|
2,50
|
2,65
|
2,80
|
3,00
|
3,15
|
3,30
|
3,45
|
3,60
|
- 0,20
|
Download of the Technical Data in PDF format.
Petersliner 3 sized
|
Papierparameter
|
 |
Toleranz
|
|
Basis weight
DIN EN ISO 536
|
g/qm
|
120
|
125
|
130
|
140
|
150
|
160
|
170
|
180
|
190
|
200
|
210
|
± 3%
|
|
Bursting resistance (Mullen tester)
|
|
275
|
290
|
300
|
320
|
340
|
370
|
390
|
410
|
430
|
460
|
480
|
- 10%
|
|
Burst factor ISO 2759
|
 |
|
  |
|
Short Span Compression
Test (SCT) CD
DIN 54 518
|
|
2,00
|
2,05
|
2,10
|
2,30
|
2,40
|
2,50
|
2,60
|
2,70
|
2,85
|
3,00
|
3,15
|
- 0,20
|
Download of the Technical Data in PDF format.
Status of the Technical Data June 2008 - We reserve the right to introduce alterations
|
 |