Petersliner White A
|
Paper parameter
|
 |
Tolerance
|
|
Area weight
DIN EN ISO 536
|
g/qm
|
125
|
130
|
140
|
± 3%
|
|
Bursting resistance (Mullen tester)
|
|
280
|
290
|
310
|
± 10
|
|
Burst factor ISO 2759
|
|
|
 |
|
Strip setup resistance (SCT) transverse
DIN 54 518
|
kN/m
|
1,85
|
1,90
|
2,05
|
± 0,20
|
|
White degree cover without UV
(ISO Brightness)
ISO 2470
|
|
78
|
- 2
|
Download of the Technical Data in PDF format.
Petersliner White B
|
Paper parameter
|
 |
Tolerance
|
|
Area weight
DIN EN ISO 536
|
g/qm
|
120
|
125
|
130
|
140
|
150
|
160
|
170
|
180
|
190
|
200
|
± 3%
|
|
Bursting resistance
(Mullen tester)
|
|
265
|
280
|
290
|
310
|
340
|
360
|
380
|
400
|
410
|
420
|
- 10
|
|
Burst factor ISO 2759
|
|
|
|
|
|
Strip setup resistance (SCT) transverse
DIN 54 518
|
kN/m
|
1,80
|
1,85
|
1,90
|
2,05
|
2,20
|
2,35
|
2,50
|
2,65
|
2,75
|
2,85
|
- 0,20
|
|
Roughness (Bendtsen)
Top Layer
DIN 53 108
|
ml/min
|
450
|
480
|
650
|
750
|
1050
|
± 10%
|
|
White degree cover without UV
(ISO Brightness)
ISO 2470
|
|
|
74
|
- 2
|
Download of the Technical Data in PDF format.
Petersliner White C
|
Paper parameter
|
 |
Tolerance
|
|
Area weight
DIN EN ISO 536
|
g/qm
|
120
|
125
|
130
|
140
|
150
|
160
|
170
|
180
|
190
|
200
|
± 3%
|
|
Bursting resistance
(Mullen tester)
|
|
265
|
280
|
290
|
310
|
340
|
360
|
380
|
400
|
410
|
420
|
- 10
|
|
Burst factor ISO 2759
|
|
|
 |
|
Strip setup resistance (SCT) transverse
DIN 54 518
|
kN/m
|
1,80
|
1,85
|
1,90
|
2,05
|
2,20
|
2,35
|
2,50
|
2,65
|
2,75
|
2,85
|
± 0,20
|
|
Roughness (Bendtsen)
Top Layer
DIN 53 108
|
ml/min
|
450
|
480
|
650
|
750
|
1050
|
± 10%
|
|
White degree cover without UV
(ISO Brightness)
ISO 2470
|
|
72
|
- 2
|
Download of the Technical Data in PDF format.
Petersliner White D
|
Paper parameter
|
 |
|
|
Tolerance
|
|
Area weight
DIN EN ISO 536
|
g/qm
|
120
|
125
|
130
|
135
|
140
|
± 3%
|
|
Bursting resistance
(Mullen tester)
|
|
250
|
270
|
280
|
290
|
300
|
- 10
|
|
Burst factor ISO 2759
|
|
|
 |
|
Strip setup resistance
(SCT) transverse
DIN 54 518
|
kN/m
|
1,65
|
1,70
|
1,75
|
1,80
|
1,85
|
- 0,20
|
|
White degree cover without UV
(ISO Brightness)
ISO 2470
|
|
70
|
- 3
|
Download of the Technical Data in PDF format.
Petersliner White mottled
|
Paper parameter
|
 |
Tolerance
|
|
Area weight
DIN EN ISO 536
|
g/qm
|
125
|
130
|
135
|
140
|
150
|
160
|
170
|
180
|
190
|
200
|
± 3%
|
|
Bursting resistance
(Mullen tester)
|
|
280
|
290
|
300
|
310
|
340
|
360
|
380
|
400
|
410
|
420
|
- 10
|
|
Burst factor ISO 2759
|
|
|
 |
|
Strip setup resistance (SCT) transverse
DIN 54 518
|
|
1,85
|
1,90
|
2,00
|
2,05
|
2,20
|
2,35
|
2,50
|
2,65
|
2,75
|
2,85
|
- 0,20
|
Download of the Technical Data in PDF format.
Status of the Technical Data January 2007 - We reserve the right to introduce alterations
|
 |